NO Glass Clips for Printrbot-solution
Description
After Running The Extruder Nozzel Into My Glass Clip, I Was Determined To Find A Better Solution. Enter Sugru, A Silicone Based Putty That Hardens Overnight, Retains Elasticity And Resists High Heat. I Simply Placed Sugru On The Edges Of The Glass Plate And Heat Bed And Let It Set Up Overnight. Now I Have A Surface With No Obstructions. I Implemented This In May 2012, And Have Used It With No Problems Since (Still Working April,2016). My Heat Bed Runs At 100 Degrees C. I Have No Affiliation With Sugru, But I Think It'S A Great Product.